产品展示

Product Center

current position: Home > Product Center > Gold and silver pearl ink

contact usContact Us

Huizhou Desikun Chemical Co., Ltd

Telephone:0752-3696596  / 3696552  / 2566848

Customer serviceQQ:2785123583 

Mailbox:hzdsksy@163.com

Address:Gate 2, New Material Industrial Park, Yonghu Town, Huiyang District, Huizhou City, Guangdong Province

Gold and silver pearl ink

Gold and silver pearl ink

  • Category:Gold and silver pearl ink
  • Browse number:
  • QR code:
  • Release time:2023-05-24 11:51:57
  • Product description

Silk screen printing gold, silver, pearl ink instruction manual

Name: Silk screen printing gold, silver, pearl ink

Model: DSK

Packing: 5KG/ barrel or 20KG/ box

1. Introduction of product features:

Laminated silver gold, silver, pearl ink series for solsol-based screen printing ink, mainly used for bank cards, credit cards and telecommunications cards and other card production, ink color flicker bright, strong metallic sense, a certain cover, suitable for PVC, PC, ABS and other sheets. The ink is suitable for large-area screen printing, stable performance, sun fast, heat resistant, lamination does not change color; The ink film can resist more than 8N tension after laminating; The product has excellent aging resistance. It is suitable for the production of high-grade cards and high standard cards.

Two: Technical parameters:


item

Parameter standard

item

Parameter standard

Appearance: (visual)

Silvery viscous liquid

Solid content: (weight loss method)

40±2

Viscosity: (cps/25℃)

2000±200

Adhesion: (3M tape)

100/100

Interlayer bond: (N)

8 N or more

Yellowing grade: (UV)

Level 4.5 or above

Shelf life: (25℃)

A year



Three: Use process:

1, printing method: screen printing: recommended 150-300 mesh screen printing, you can use our DSK783 to adjust the viscosity.

2, drying method: infrared drying: at the temperature of 80℃-100℃ drying time is 30-40 seconds, air cooling time is 10-20 seconds

When the temperature is 50℃-55℃, the drying time is 15-20 minutes, and the air cooling time is 10-15 minutes.

3, laminating requirements: laminating temperature 130-150℃, hot laminating time 18-23 minutes, cold pressing time 15-20 minutes, laminating pressure does not exceed 11Mpa.


Iv. Precautions:

1. Please stir well before use (try to use mixing equipment: 3-5 minutes is appropriate).

2. If the ink is found to be thickened or the fluidity is poor during the use of the ink, please add an appropriate amount of diluent + ink oil 2871=1:1 dilution (the addition amount should not be higher than 20%), and fully stir evenly.

3. If the product accidentally touches the skin or spills into the eyes, please clean it immediately with plenty of water. In serious cases, please seek medical attention in time.

4. This product should be stored in a cool and ventilated place, away from fire.

5. The data listed in this product is based on the results obtained by our current laboratory and some customers. Due to the influence of customers' conditions and methods of use, the results will be different, so the content listed in this product does not make any guarantee for reference only.




Recently Viewed:

Site map | RSS | XML Filing number:粤ICP备2021013258号 Technical Support:华信环球